LabAdviser/Technology Research/Fabrication of Hyperbolic Metamaterials using Atomic Layer Deposition: Difference between revisions
| Line 11: | Line 11: | ||
[[image:Evgeniys project description.jpg|400px|thumb|Figur 1 Schematics of (a) a multilayer and (b) a nanowire hyperbolic metamaterial.]] | [[image:Evgeniys project description.jpg|400px|thumb|Figur 1 Schematics of (a) a multilayer and (b) a nanowire hyperbolic metamaterial.]] | ||
Recent years have shown an explosive interest in the physics of hyperbolic metamaterials (HMMs). Electrodynamically HMMs are described by a dielectric permittivity tensor (ε) with components of opposite signs (e.g. εx=εy<0, εz>0). In such media the unusual hyperbolic dispersion relation supports propagating waves with anomalously large wave vectors. This and related phenomena give rise to a multitude of exotic physical effects and promising applications. Examples include broadband spontaneous emission enhancement, far-field subwavelength imaging (so-called hyperlensing) and anomalous heat transfer capabilities. | Recent years have shown an explosive interest in the physics of hyperbolic metamaterials (HMMs). Electrodynamically HMMs are described by a dielectric permittivity tensor (ε) with components of opposite signs (e.g. εx=εy<0, εz>0). In such media the unusual hyperbolic dispersion relation supports propagating waves with anomalously large wave vectors. This and related phenomena give rise to a multitude of exotic physical effects and promising applications. Examples include broadband spontaneous emission enhancement, far-field subwavelength imaging (so-called hyperlensing) and anomalous heat transfer capabilities. | ||
From the fabrication standpoint, HMMs turn out to be deceptively simple: a typical geometry consists of a repeated basic metal-dielectric bilayer stack or a lattice of metallic nanowires embedded in a dielecric matrix. However, for the salient HMM properties to be pronounced, ultrathin, nanometer-scale thicknesses are required. | From the fabrication standpoint, HMMs turn out to be deceptively simple: a typical geometry consists of a repeated basic metal-dielectric bilayer stack or a lattice of metallic nanowires embedded in a dielecric matrix. However, for the salient HMM properties to be pronounced, ultrathin, nanometer-scale thicknesses are required.<br> | ||
The required high-quality ultrathin layers (around 10 nm) can be fabricated using atomic layer deposition (ALD). ALD is a cyclic self-limiting thin film deposition technology allowing molecule level thickness control. As the deposition relies on a surface reaction, conformal pinhole free films can be deposited. | The required high-quality ultrathin layers (around 10 nm) can be fabricated using atomic layer deposition (ALD). ALD is a cyclic self-limiting thin film deposition technology allowing molecule level thickness control. As the deposition relies on a surface reaction, conformal pinhole free films can be deposited.<br> | ||
The main challenge of implementation of ALD processing for HMM fabrication is the requirement for depositing alternating layers of metals (Ag, Cu, W) and dielectric spacers (alumina, titania, silica) . Required thicknesses are in the range 5-15 nm for metals and 10-20 nm for dielectrics (oxides).<br clear="all" /> | The main challenge of implementation of ALD processing for HMM fabrication is the requirement for depositing alternating layers of metals (Ag, Cu, W) and dielectric spacers (alumina, titania, silica) . Required thicknesses are in the range 5-15 nm for metals and 10-20 nm for dielectrics (oxides).<br clear="all" /> | ||
Revision as of 09:13, 11 February 2016
Feedback to this page: click here
Fabrication of Hyperbolic Metamaterials using Atomic Layer Deposition
- Project type: Ph.d project
- Project responsible: Evgeniy Shkodin
- Supervisors: Andrei Lavrinenko, Flemming Jensen
- Partners involved: DTU Fotonik, DTU Danchip
Project Description

Recent years have shown an explosive interest in the physics of hyperbolic metamaterials (HMMs). Electrodynamically HMMs are described by a dielectric permittivity tensor (ε) with components of opposite signs (e.g. εx=εy<0, εz>0). In such media the unusual hyperbolic dispersion relation supports propagating waves with anomalously large wave vectors. This and related phenomena give rise to a multitude of exotic physical effects and promising applications. Examples include broadband spontaneous emission enhancement, far-field subwavelength imaging (so-called hyperlensing) and anomalous heat transfer capabilities.
From the fabrication standpoint, HMMs turn out to be deceptively simple: a typical geometry consists of a repeated basic metal-dielectric bilayer stack or a lattice of metallic nanowires embedded in a dielecric matrix. However, for the salient HMM properties to be pronounced, ultrathin, nanometer-scale thicknesses are required.
The required high-quality ultrathin layers (around 10 nm) can be fabricated using atomic layer deposition (ALD). ALD is a cyclic self-limiting thin film deposition technology allowing molecule level thickness control. As the deposition relies on a surface reaction, conformal pinhole free films can be deposited.
The main challenge of implementation of ALD processing for HMM fabrication is the requirement for depositing alternating layers of metals (Ag, Cu, W) and dielectric spacers (alumina, titania, silica) . Required thicknesses are in the range 5-15 nm for metals and 10-20 nm for dielectrics (oxides).
Publications
Name of publication1 made in this project
Reference and link to the publication
- Link Process flow(s) relevant to this publication
- Link(s) to Process development made in connection to this publication this is decribes in either LabAdviser or Process2Share.
Name of publication2 made in this project
Reference and link to the publication
- Link Process flow(s) relevant to this publication
- Link(s) to Process development made in connection to this publication this is decribes in either LabAdviser or Process2Share.
Name of publication3 made in this project
Reference and link to the publication
- Link Process flow(s) relevant to this publication
- Link(s) to Process development made in connection to this publication this is decribes in either LabAdviser or Process2Share.