Specific Process Knowledge/Thin film deposition/Cluster-based multi-chamber high vacuum sputtering deposition system: Difference between revisions
Appearance
| Line 212: | Line 212: | ||
== Sputter-System Metal-Nitride (PC3) == | == Sputter-System Metal-Nitride (PC3) == | ||
The second process chamber called PC3 consists of two KJLC Torus® 3" magnetron sputtering sources and one height adjustable KJLC Torus® 4" magnetron sputtering source, also with possibility of RF, DC, Pulse DC and HIPIMS sputtering. The chamber has a possibility to do the RF bias on a substrate, which can be used as substrate cleaning before the deposition or used during the deposition to alter the film properties. | The second process chamber called PC3 consists of two KJLC Torus® 3" magnetron sputtering sources and one height adjustable KJLC Torus® 4" magnetron sputtering source, also with possibility of RF, DC, Pulse DC and HIPIMS sputtering. The chamber has a possibility to do the RF bias on a substrate, which can be used as substrate cleaning before the deposition or used during the deposition to alter the film properties. It is possible to do the co-sputtering (sputtering of two or more sources at the same time) as long as the sources are not sharing the same power supply. | ||
<gallery caption=" | <gallery caption="Process chamber PC 3" widths="600px" heights="600px" perrow="2"> | ||
image:PC3_photo.png| | image:PC3_photo.png| Photography of the chamber. | ||
image:PC3_during_sputtering.png| Deposition | image:PC3_during_sputtering.png| Deposition from source 2. | ||
</gallery> | </gallery> | ||