==Project Description==
==Project Description==
[[image:HMM_implementation_topology.png|600px|thumb|Figur 1. Schematics of (a) a multilayer and (b) a nanowire hyperbolic metamaterial.]]


The aim of this Ph.D. project is to obtain a deeper understanding of the interaction at the nanoscale level between ultra-thin metal films used in micro/nanofabrication, exploiting the unique capabilities of thin-film fabrication and characterization offered by the combination of the DTU Danchip/Cen facilities.
The aim of this Ph.D. project is to obtain a deeper understanding of the interaction at the nanoscale level between ultra-thin metal films used in micro/nanofabrication, exploiting the unique capabilities of thin-film fabrication and characterization offered by the combination of the DTU Danchip/Cen facilities.