Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Silicon Nitride/Deposition of Silicon Nitride using PECVD: Difference between revisions

Bghe (talk | contribs)
Bghe (talk | contribs)
Line 194: Line 194:




==Recipes on PECVD1 for deposition of silicon nitride and silicon oxynitride PECVD1 has been decommissioned==
==Recipes on PECVD1 for deposition of silicon nitride and silicon oxynitride. <span style="color:Red">Expired!</span>:PECVD1 has been decommissioned==
===Recipes===
===Recipes===
{| border="1" cellspacing="0" cellpadding="7"