==Organic Ice Resists== | ==Organic Ice Resists== | ||
[[File:Comparison1_OIR.PNG|400px]] | |||
Vapour pressure is the tabulated value at room temperature. Freezing temperature is the tabulated value at atmospheric pressure. | |||
[[File:Comparison2_OIR.PNG|400px]] | |||
Thickness ranges are suggestions based on our experience, and are measured after sublimation via AFM. | |||
==Contrast Curve== | ==Contrast Curve== | ||
[[File:Contrast_OIR.png|600px]] | |||
==Multi-layers== | ==Multi-layers== | ||