LabAdviser/Technology Research/Fabrication of Hyperbolic Metamaterials using Atomic Layer Deposition: Difference between revisions
Appearance
mNo edit summary |
|||
| (42 intermediate revisions by 3 users not shown) | |||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/LabAdviser/Technology_Research/Fabrication_of_Hyperbolic_Metamaterials_using_Atomic_Layer_Deposition click here]''' | ||
<i>This page is written by <b>Evgeniy Shkondin @DTU Nanolab</b> if nothing else is stated. <br> | |||
All images and photos on this page belongs to <b>DTU Nanolab</b> and <b>DTU Electro</b> (previous DTU Fotonik).<br> | |||
The fabrication and characterization described below were conducted in <b>2013-2016 by Evgeniy Shkondin, DTU Nanolab</b>.<br></i> | |||
=Fabrication of Hyperbolic Metamaterials using Atomic Layer Deposition= | =Fabrication of Hyperbolic Metamaterials using Atomic Layer Deposition= | ||
*'''Project type:''' Ph.d project | *'''Project type:''' Ph.d project | ||
*'''Project responsible:''' | *'''Project responsible: Evgeniy Shkondin <br> [[image:orcid_16x16.png|16x16px]]https://orcid.org/0000-0002-8347-1814''' | ||
*'''Supervisors:''' Andrei Lavrinenko, Flemming Jensen | *'''Supervisors:''' Andrei Lavrinenko, Flemming Jensen | ||
*'''Partners involved:''' DTU Fotonik, DTU Danchip | *'''Partners involved:''' DTU Fotonik, DTU Nanolab (former DTU Danchip) | ||
*'''Full Thesis:''' https://orbit.dtu.dk/en/publications/fabrication-of-hyperbolic-metamaterials-using-atomic-layer-deposi | |||
==Project Description== | ==Project Description== | ||
| Line 49: | Line 55: | ||
==Publications in peer-review journals== | ==Publications in peer-review journals== | ||
===Midinfrared Surface Waves on a High Aspect Ratio Nanotrench Platform === | |||
O. Takayama, <u>E. Shkondin</u>, A. Bogdanov, M. E. Aryaee Panah, K. Golenicki, P. Dmitriev, T. Repän, R. Malureanu, P. Belov, F. Jensen & A. Lavrinenko. ACS Photonics, 2017, 4 (11), pp 2899–2907 [http://pubs.acs.org/doi/abs/10.1021/acsphotonics.7b00924 LINK] | |||
*[[/AZO_gratings|<strong>Procces flow</strong>]] | |||
* | ===Large-Scale High Aspect Ratio Al-Doped ZnO Nanopillars Arrays as Anisotropic Metamaterials=== | ||
<u>E. Shkondin</u>, O. Takayama, M. E. Aryaee Panah, P. Liu, P. V. Larsen, M. D. Mar, F. Jensen. & A. Lavrinenko | |||
(2017). Optical Materials Express, 7(5), pp. 1606-1627 (2017) [https://www.osapublishing.org/ome/abstract.cfm?uri=ome-7-5-1606 LINK] | |||
*[[/AZO_pillars|<strong>Procces flow</strong>]] | |||
===Laguerre-Gauss Beam Generation in IR and UV by Subwavelength Surface-Relief Gratings=== | ===Laguerre-Gauss Beam Generation in IR and UV by Subwavelength Surface-Relief Gratings=== | ||
L. Vertchenko, <u>E. Shkondin</u>, R. Malureanu, & C. Monken | |||
(2017) | (2017). Optics Express, 25(6), pp. 5917-5926 (2017) [https://osapublishing.org/oe/abstract.cfm?uri=oe-25-6-5917 LINK] | ||
*[[/TiO2_Q_plates|Procces flow]] | *[[/TiO2_Q_plates|<strong>Procces flow</strong>]] | ||
===Fabrication of High Aspect Ratio TiO<sub>2</sub> and Al<sub>2</sub>O<sub>3</sub> Nanogratings by Atomic Layer Deposition=== | ===Fabrication of High Aspect Ratio TiO<sub>2</sub> and Al<sub>2</sub>O<sub>3</sub> Nanogratings by Atomic Layer Deposition=== | ||
<u> | <u>E. Shkondin</u>, O. Takayama, J. Lindhard, P. V. Larsen, M. D. Mar, F. Jensen & A. Lavrinenko | ||
(2016) | (2016). Journal of Vacuum Science and Technology A, 34, 031605 (2016) [http://scitation.aip.org/content/avs/journal/jvsta/34/3/10.1116/1.4947586 LINK] | ||
*[[/TIO_ALU_Gratings_Procces_flow|Procces flow]] | *[[/TIO_ALU_Gratings_Procces_flow|<strong>Procces flow</strong>]] | ||
===Experimental Demonstration of Effective Medium Approximation Breakdown in Deeply Subwavelength All-Dielectric Multilayers=== | ===Experimental Demonstration of Effective Medium Approximation Breakdown in Deeply Subwavelength All-Dielectric Multilayers=== | ||
S. Zhukovsky, A. Andryieuski, O. Takayama, <u>E. Shkondin</u>, R. Malureanu, F. Jensen, & A. Lavrinenko | |||
(2015) | (2015). Physical Review Letters, 115(17), 177402 [http://journals.aps.org/prl/abstract/10.1103/PhysRevLett.115.177402 LINK] | ||
*[[/EMT_Procces_flow|<strong>Procces flow</strong>]] | |||
<br> | |||
==Publications in proceedings== | |||
===Effective medium approximation for deeply subwavelength all-dielectric multilayers: when does it break down?=== | |||
A. Lavrinenko, S. Zhukovsky, A. Andryieuski, O. Takayama, <u>E. Shkondin</u>, R. Malureanu and F. Jensen <br> | |||
Proceedings of SPIE. Vol. 9883 SPIE - International Society for Optical Engineering, (2016) | |||
===Fabrication of deep-profile Al-doped ZnO one- and two-dimensional lattices as plasmonic elements=== | |||
F. Jensen, <u>E. Shkondin</u>, O. Takayama, P. V. Larsen, M. D. Mar, R. Malureanu, A. V. Lavrinenko <br> | |||
Proceedings of SPIE. Vol. 9921 SPIE - International Society for Optical Engineering, (2016) | |||
===Hyperbolic metamaterials with complex geometry=== | |||
A. V. Lavrinenko, A. Andryieuski, S. Zhukovsky, O. Takayama, <u>E. Skhondin</u>, M. E. Aryaee Panah, R. Malureanu, F. Jensen <br> | |||
META'16, The 6th International Conference on Metamaterials, Photonic Crystals and Plasmonics, Malaga, Spain, 2A23, Proceedings, p.471-472 (2016) | |||
===Surface waves on metal-dielectric metamaterials=== | |||
O. Takayama, <u>E. Shkondin</u>, M. E. Aryaee Panah, T. Repän, R. Malureanu, F. Jensen, A. V. Lavrinenko <br> | |||
Proceedings of 18th International Conference on Transparent Optical Networks. IEEE, (2016) | |||
===Surface waves on metamaterials interfaces=== | |||
O. Takayama, <u>E. Shkondin</u>, M. E. Aryaee Panah, T. Repän, R. Malureanu, F. Jensen, A. V. Lavrinenko <br> | |||
Proceedings of 10th International Congress on Advanced Electromagnetic Materials in Microwaves and Optics.(2016) | |||
===Ultra-thin metal and dielectric layers for nanophotonic applications=== | |||
<u>E. Shkondin</u>, L. Leandro, R. Malureanu, F. Jensen, N. Rozlosnik, A. V. Lavrinenko <br> | |||
Proceedings of ICTON, IEEE, 7193380. (2015) | |||
==Conferences and workshops== | |||
===Conductive oxides trench structures as hyperbolic metamaterials in mid-infrared range=== | |||
O. Takayama, <u>E. Shkondin</u>, M. E. A. Panah, T. Reän, R. Malureanu, F. Jensen, A. V. Lavrinenko <br> | |||
2016. Abstract from 14th International Conference of Near-Field Optics, Nanophotonics and Related Techniques, Hamamatsu, Japan | |||
===Fabrication of hollow coaxial ZnAl<sub>2</sub>O<sub>4</sub> high aspect ratio freestanding nanopillars based on the Kirkendall effect=== | |||
<u>E. Shkondin</u>, F. Jensen, A. V. Lavrinenko <br> | |||
2016. Abstract from 42nd Micro and Nano Engineering 2016, Vienna, Austria | |||
===Fabrication of Al-doped ZnO high aspect ratio nanowires and trenches as active components in mid-infrared plasmonics=== | |||
<u>E. Shkondin</u>, O. Takayama, P. V. Larsen, M. D. Mar, F. Jensen, A. V. Lavrinenko <br> | |||
2016. Abstract from 16th Atomic Layer Deposition Conference, Dublin, Ireland. | |||
===TiO<sub>2</sub> and Al<sub>2</sub>O<sub>3</sub> ALD grown multilayers for subwavelength photonics=== | |||
<u>E. Shkondin</u>, F. Jensen, A. V. Lavrinenko, M. D. Mar, P. V. Larsen, R. Malureanu, S. Zhukovsky, A. Andryieuski, O. Takayama <br> | |||
2015. DTU's Sustain Conference 2015, Technical University of Denmark, Kgs. Lyngby, Denmark (2015) | |||
===Deep subwavelength photonic multilayers fabricated by atomic layer deposition=== | |||
<u>E. Shkondin</u>, S. Zhukovsky, A. Andryieuski, O. Takayama, R. Malureanu, M. D. Mar, A. V. Lavrinenko, F. Jensen <br> | |||
2015. Paper presented at 41st International conference on Micro and Nano Engineering, The Hague, Netherlands. | |||
===Fabrication of TiO<sub>2</sub> and Al<sub>2</sub>O<sub>3</sub> High Aspect Ratio Nanostructured Gratings at Sub-Micrometer Scale=== | |||
<u>E. Shkondin</u>, J. M. Lindhard, M. D. Mar, F. Jensen, A. V. Lavrinenko <br> | |||
2015. Paper presented at 15th International Conference on Atomic Layer Deposition, Portland, Oregon, United States | |||
===Depositing Materials on the Micro- and Nanoscale=== | |||
M. D. Mar, B. Herstrøm, <u>E. Shkondin</u>, P. Pholprasit, F. Jensen <br> | |||
2014. DTU's Sustain Conference 2014, Technical University of Denmark, Kgs. Lyngby, Denmark (2014) | |||
<!-- This is a comment --> | <!-- This is a comment --> | ||
<!-- This is a comment --> | <!-- This is a comment --> | ||