*Reversal bake time: 60-120 s
*Reversal bake time: 60-120 s
*Flood exposure: 200-500 mJ/cm<sup>2</sup>
*Flood exposure: 200-500 mJ/cm<sup>2</sup>


If 5214E is baked after exposure, the exposed resist will cross-link, making it insoluble in the developer. This is called the "Reversal bake", or sometimes the post-exposure bake. The reversal bake activates cross-linking of the exposed areas, which "reverses" the polarity of the design.