Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange/polySi/Cpoly4: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 23: | Line 23: | ||
| Pegasus/jmli | | Pegasus/jmli | ||
| 10 minute TDESC clean + 45 sec barc etch | | 10 minute TDESC clean + 45 sec barc etch | ||
| | | nanolab/jml/showerhead/Cpoly4, 20 cycles or 2:16 minutes | ||
| S004733 | | S004733 | ||
| New showerhead | | New showerhead | ||