Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1/1Open: Difference between revisions

Jmli (talk | contribs)
Created page with " ds"
 
Jmli (talk | contribs)
No edit summary
Line 1: Line 1:
ds
= Prepare the spectra for analysis =
 
Double click on the ''Experiment 2.VGX'' file and Avantage should start. If you open from Avantage, remember to select 'All files *.*' to be able to find the *.VGX file.
 
[[File:ALD-Sandwich-01.jpg|700px]]
 
The experiment has three points. Here, we will process the data in the 'Scanned' point. Minimize the other points and open a new processing grid.
 
[[File:ALD-Sandwich-03.jpg|700px]]
 
Click on the point in the experiment tree and drag the content into the processing grid.
 
[[File:ALD-Sandwich-04a.jpg|700px]]
 
This action will create a grid with all spectra. Here, however, we will remove the survey spectrum from the processing grid by deleting it (keep in mind always to separate processing grids for [[Specific Process Knowledge/Characterization/XPS/Processing/Guidelines|survey spectra, scanned and snapshot spectra]]).
 
 
[[File:ALD-Sandwich-06.jpg|700px]]
 
Rearrange the scanned spectra in the processing grid (Here called 'Data Grid2') with the button highlighted to the right.
 
[[File:ALD-Sandwich-09a.jpg|700px]]
 
Open a new processing grid for the survey spectra, drag the spectra over there and remove the remaining empty grids. Here, the processing grid is called 'Data Grid3'.
 
[[File:ALD-Sandwich-12.jpg|700px]]
 
Now, we have two processing grids ready for analysis.