30 March 2011

  • curprev 15:0215:02, 30 March 2011 Jml talk contribs 189 bytes +189 Etching of nanostructures in Si using DRIE-Pegasus: nano1.3 recipe, Run ID 1856 (a) and 1857 (a+b), time 60 secs (a) and 120 secs (b), SF6 38, C4F8 52, 4mtorr, 600/40 coil/platen, -10 degs.