  • curprev 15:0715:07, 30 March 2011 Jml talk contribs 1,372 bytes +1,372 New page: == The nano1.3 recipe == {| border="2" cellpadding="2" cellspacing="1" |+ '''Recipe nano1.3''' |- ! rowspan="6" align="center"| Recipe | Gas | C<sub>4</sub>F<sub>8</sub> 38 sccm, SF<sub>...