|Dopants introduced by diffusion from gas-phase (POCl<sub>3</sub>). A thin phosphorous glass is formed on the substrate and phosphorous atoms are driven in. The phosphorous glass is afterward removed by a short BHF etch. Often further annealing is desired in order to redistribute the dopants in the material. This is done at 800°C - 1150°C in either high temperature annealing furnaces or by rapid thermal annealing. | |Dopants introduced by diffusion from gas-phase (POCl<sub>3</sub>). A thin phosphorous glass is formed on the substrate and phosphorous atoms are driven in. The phosphorous glass is afterward removed by a short BHF etch. Often further annealing is desired in order to redistribute the dopants in the material. This is done at 800°C - 1150°C in either high temperature annealing furnaces or by rapid thermal annealing. | ||
|Dopants introduced by diffusion from solid source wafers containing B<sub>2</sub>O<sub>3</sub>. A boron glass is formed on the substrate and boron atoms are driven in. The boron glass is afterward removed by a | |Dopants introduced by diffusion from solid source wafers containing B<sub>2</sub>O<sub>3</sub>. A boron glass is formed on the substrate and boron atoms are driven in. The boron glass is afterward removed by a low temperature oxidation process (1 hour at 800°C-900°C) in the boron drive in furnace (A1) followed by a BHF etch. Often further annealing is desired in order to redistribute the dopants in the material. This is done at 800°C - 1150°C in either high temperature annealing furnaces or by rapid thermal annealing. | ||
|Deposition of doped thin film (oxides or nitrides). A high temperature step to drive in and redistribute the dopants in the material is required. This is typically done at 800°C - 1150°C in either high temperature annealing furnaces (C1 or C3) or by rapid thermal annealing. The doped glass can afterwards be removed in a BHF etch. | |Deposition of doped thin film (oxides or nitrides). A high temperature step to drive in and redistribute the dopants in the material is required. This is typically done at 800°C - 1150°C in either high temperature annealing furnaces (C1 or C3) or by rapid thermal annealing. The doped glass can afterwards be removed in a BHF etch. | ||
|Dopants introduced by in-situ doping of poly/amorphous Si. In some cases you need a high temperature step to redistribute the dopants in the material and alter the crystallinity. This is typically done at 800°C - 1150°C in either high temperature annealing furnaces (C1 or C3) or by rapid thermal annealing. | |Dopants introduced by in-situ doping of poly/amorphous Si. In some cases you need a high temperature step to redistribute the dopants in the material and alter the crystallinity. This is typically done at 800°C - 1150°C in either high temperature annealing furnaces (C1 or C3) or by rapid thermal annealing. |
Revision as of 16:04, 31 October 2014
THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here
Doping your wafer
This page is about doping your wafer or making a thin film layer doped with boron, phosphorous or Germanium.
- Dope with Phosphorous - Doping Silicon wafers with phosphorous by thermal predeposition and drive-in
- Dope with Boron - Doping Silicon wafers with boron by thermal predeposition and drive-in
- Furnace LPCVD PolySilicon - Deposition of PolySi doped with B or P
- PECVD - Making boron glass (BSG), phosphorus glass (PSG), boron-phosphorous glass PBSG or germanium doped glass
- Ion implantation
Comparison of different doping processes
Phosphorous predep | Boron predep | PECVD doped thin film | Doped Poly Si | |
---|---|---|---|---|
Generel description | Dopants introduced by diffusion from gas-phase (POCl3). A thin phosphorous glass is formed on the substrate and phosphorous atoms are driven in. The phosphorous glass is afterward removed by a short BHF etch. Often further annealing is desired in order to redistribute the dopants in the material. This is done at 800°C - 1150°C in either high temperature annealing furnaces or by rapid thermal annealing. | Dopants introduced by diffusion from solid source wafers containing B2O3. A boron glass is formed on the substrate and boron atoms are driven in. The boron glass is afterward removed by a low temperature oxidation process (1 hour at 800°C-900°C) in the boron drive in furnace (A1) followed by a BHF etch. Often further annealing is desired in order to redistribute the dopants in the material. This is done at 800°C - 1150°C in either high temperature annealing furnaces or by rapid thermal annealing. | Deposition of doped thin film (oxides or nitrides). A high temperature step to drive in and redistribute the dopants in the material is required. This is typically done at 800°C - 1150°C in either high temperature annealing furnaces (C1 or C3) or by rapid thermal annealing. The doped glass can afterwards be removed in a BHF etch. | Dopants introduced by in-situ doping of poly/amorphous Si. In some cases you need a high temperature step to redistribute the dopants in the material and alter the crystallinity. This is typically done at 800°C - 1150°C in either high temperature annealing furnaces (C1 or C3) or by rapid thermal annealing. |
Process Temperature |
|
|
|
|
Dopant |
|
|
|
|
Substrate size |
|
|
|
|
Allowed materials |
|
|
|
|
Ion implantation
Ion implantation cannot be done at Danchip. IBS offers ion-beam implantation as a service. See more at the homepage of IBS: http://www.ion-beam-services.com/about_us.htm