Specific Process Knowledge/Thermal Process/Oxidation/Oxidation on III-V oxidation furnace (C2)

From LabAdviser

THIS PAGE IS UNDER CONSTRUCTION

Flow440 recipe

Standby: N2 purge at 3 SLM and Standby temperature at 440C

LM-LOCK: Check LabManager

Wet stabilize: N2 through bubbler at 1.5 SLM for 20 min and then wait for operator to open the furnace

Open

Load samples

Close

Wet oxidation: Time: variable

Open Automatically opens after the oxidation time reaches

Unload samples