Specific Process Knowledge/Thermal Process/Oxidation/Oxidation on III-V oxidation furnace (C2)
Jump to navigation
Jump to search
THIS PAGE IS UNDER CONSTRUCTION
Flow440 recipe
Standby:N2 purge at 3 SLM and Standby temperature at 440C
LM-LOCK: Check LabManager
Wet stabilize: N2 through bubbler at 1.5 SLM
Time: 20 min Wait for operator
Open Load samples Close
Wet oxidation Time: variable
Open Unload samples