= New recipes=
= New recipes=


The idea of int
It was professor [https://www.dtu.dk/service/telefonbog/person?id=103402&cpid=191195&tab=1 Henri Jansen] at DTU Nanolab who came up with the idea of adding the Picoscope to the Pegasi tools. Since then his group has researched a lot into its possibilities. Below is a list of publications in which the Picoscope plays a crucial role:  
The finetuning of Bosch recipes made possible by the picoscope has been researched a lot by the group of professor [https://www.dtu.dk/service/telefonbog/person?id=103402&cpid=191195&tab=1 Henri Jansen] at DTU Nanolab. Below is a list of publications:  
*[[:file:DREM1.pdf | Bingdong Chang et al.: DREM: Infinite etch selectivity and optimized scallop size distribution with conventional photoresists in an adapted multiplexed Bosch DRIE process]]
*[[:file:DREM1.pdf | Bingdong Chang et al.: DREM: Infinite etch selectivity and optimized scallop size distribution with conventional photoresists in an adapted multiplexed Bosch DRIE process]]
*[[:file:DREM2.pdf | Bingdong Chang et al.: DREM2: a facile fabrication strategy for freestanding three dimensional silicon micro- and nanostructures by a modified Bosch etch process]]
*[[:file:DREM2.pdf | Bingdong Chang et al.: DREM2: a facile fabrication strategy for freestanding three dimensional silicon micro- and nanostructures by a modified Bosch etch process]]