'''Flow440''' recipe | =='''Flow440''' recipe== | ||
Standby: N2 purge at 3 SLM and Standby temperature at 440C | '''Standby''': N2 purge at 3 SLM and Standby temperature at 440C | ||
LM-LOCK: Check LabManager | LM-LOCK: Check LabManager |
Revision as of 15:31, 16 August 2019
THIS PAGE IS UNDER CONSTRUCTION
Flow440 recipe
Standby: N2 purge at 3 SLM and Standby temperature at 440C
LM-LOCK: Check LabManager
Wet stabilize: N2 through bubbler at 1.5 SLM for 20 min and then wait for operator to open the furnace
Open
Load samples
Close
Wet oxidation: Time: variable
Open
Unload samples