Specific Process Knowledge/Lithography/Espacer: Difference between revisions
No edit summary |
No edit summary |
||
Line 59: | Line 59: | ||
|-style="background:WhiteSmoke; text-align:center; color:black" | |-style="background:WhiteSmoke; text-align:center; color:black" | ||
|Nikon ECLIPSE optical microscope, E-5 | |Nikon ECLIPSE optical microscope, E-5 | ||
|[[File: | |[[File:NoEspacerOverview.png|300px]] | ||
|[[File:ESPACERoverview.png|300px]] | |[[File:ESPACERoverview.png|300px]] | ||
|- | |- | ||
Line 65: | Line 65: | ||
|-style="background:WhiteSmoke; text-align:center; color:black" | |-style="background:WhiteSmoke; text-align:center; color:black" | ||
|Nikon ECLIPSE optical microscope, E-5 | |Nikon ECLIPSE optical microscope, E-5 | ||
|[[File: | |[[File:NoEspacerOverviewBasedose.png|300px]] | ||
|[[File:ESPACERbasedose.png|300px]] | |[[File:ESPACERbasedose.png|300px]] | ||
|- | |- | ||
Line 71: | Line 71: | ||
|-style="background:WhiteSmoke; text-align:center; color:black" | |-style="background:WhiteSmoke; text-align:center; color:black" | ||
|Nikon ECLIPSE optical microscope, E-5 | |Nikon ECLIPSE optical microscope, E-5 | ||
|[[File: | |[[File:noEspacerBasedose-5%.png|300px]] | ||
| | | | ||
|- | |- |
Revision as of 11:32, 10 July 2014
We have Espacer in stock and approved for use in the cleanroom. You can find a guideline for a process flow here: Process_Flow_ZEP_ESPACER.docx. Technical information of Espacer can be found here: Espacer_300_Technical_Info.pdf, Espacer_catalog.pdf.
Please contact Lithography if you wish to test this material.
Process | No ESPACER | ESPACER |
---|---|---|
Resist | AR-P 6200/2 AllResist E-beam resist | |
Spin Coat | 1 min @ 4000 rpm, softbake 2 min @ 150 degC, thickness ~140nm | |
ESPACER | 1 min @ 2000 rpm (no softbake), Manual Spinner 1 (Laurell) | |
E-beam exposure | 2 nA, aperture 5, dose 150-310 muC/cm2, SHOT A,10 | |
Rinse | Rinsed with hand shower in fumehood, dried with N2 gun | |
Developing | SX-AR 600-54/6 60 sec, 60 sec IPA rinse | |
Characterization | ||
Nikon ECLIPSE optical microscope, E-5 | ||
Nikon ECLIPSE optical microscope, E-5 | ||
Nikon ECLIPSE optical microscope, E-5 | ||
Sputter Coated | <10nm Pt at DTU CEN | |
Zeiss SEM supra 60VP, D-2 | 230 muC/cm2 |