Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Titanium: Difference between revisions

From LabAdviser
Kn (talk | contribs)
No edit summary
Knil (talk | contribs)
Line 57: Line 57:
|-
|-
|-style="background:WhiteSmoke; color:black"
|-style="background:WhiteSmoke; color:black"
!Allowed materials
|
* Silicon oxide
* Silicon (oxy)nitride
* Photoresist
* PMMA
* Mylar
* SU-8
* Metals
|
* Silicon oxide
* Silicon (oxy)nitride
* Photoresist
* PMMA
* Mylar
* SU-8
* Metals
|
* Silicon oxide
* Silicon (oxy)nitride
* Photoresist
* PMMA
* Mylar
* SU-8
* Metals
|
* Silicon oxide
* Silicon (oxy)nitride
* Photoresist
* PMMA
* Mylar
* SU-8
* Metals
|-style="background:LightGrey; color:black"
! Comment
! Comment
|
|
Line 63: Line 97:
|
|
|-
|-
|-style="background:WhiteSmoke; color:black"


|}
|}


== Comments: Choise of equipment ==
== Comments: Choise of equipment ==

Revision as of 12:01, 28 January 2014

Feedback to this page: click here


Titanium deposition

Titanium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.


E-beam evaporation (Alcatel) E-beam evaporation (Wordentec) E-beam evaporation (PVD co-sputter/evaporation) Sputter deposition (Wordentec)
Batch size
  • Up to 1x4" wafers
  • smaller pieces
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
  • 12x2" wafers or
  • 12x4" wafers or
  • 4x6" wafers
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
Pre-clean RF Ar clean RF Ar clean RF Ar clean RF Ar clean
Layer thickness 10Å to 1µm 10Å to 1 µm 10Å to 1000Å .
Deposition rate 2Å/s to 15Å/s 10Å/s to 15Å/s About 1Å/s Depending on process parameters, see here.
Allowed materials
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
Comment Only very thin layers (up to 100nm).

Comments: Choise of equipment

Thick layers

Comments: Adhesion layer

Ti as adhesion layer