==Titanium deposition ==


Titanium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
Titanium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.

Revision as of 12:40, 1 March 2013

Feedback to this page: click here


Titanium deposition

Titanium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.


E-beam evaporation (Alcatel) E-beam evaporation (Wordentec) E-beam evaporation (PVD co-sputter/evaporation) Sputter deposition (Wordentec)
Batch size
  • Up to 1x4" wafers
  • smaller pieces
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
  • 12x2" wafers or
  • 12x4" wafers or
  • 4x6" wafers
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
Pre-clean RF Ar clean RF Ar clean RF Ar clean RF Ar clean
Layer thickness 10Å to 1µm 10Å to 1 µm 10Å to 1000Å .
Deposition rate 2Å/s to 15Å/s 10Å/s to 15Å/s About 1Å/s Depending on process parameters, see here.


Comments: Choise of equipment

Thick layers

Comments: Adhesion layer

Ti as adhesion layer