Specific Process Knowledge/Lithography/Espacer: Difference between revisions
Created page with "We have ESPACER in stock and approved for use in the cleanroom. You can find a guideline for a process flow here: [[media:Process_Flow_ZEP_ESPACER.docx|Process_Flow_ZEP_ESP..." |
No edit summary |
||
Line 38: | Line 38: | ||
|- | |- | ||
|- | |||
|-style="background:WhiteSmoke; text-align:center; color:black" | |||
|Rinse | |||
| | |||
|Rinsed with hand shower in fumehood, dried with N2 gun | |||
|- | |||
|- | |- |
Revision as of 09:21, 10 July 2014
We have ESPACER in stock and approved for use in the cleanroom. You can find a guideline for a process flow here: Process_Flow_ZEP_ESPACER.docx. Technical information of EPSCAER can be found here: Espacer_300_Technical_Info.pdf, Espacer_catalog.pdf.
Please contact Lithography if you wish to test this material.