Specific Process Knowledge/Thermal Process/Oxidation/Oxidation on III-V oxidation furnace (C2): Difference between revisions

From LabAdviser
Jump to navigation Jump to search
(Created page with "=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>=")
 
No edit summary
 
(8 intermediate revisions by 2 users not shown)
Line 1: Line 1:
=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>=
=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>=
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i>
The furnace is being tested.
=='''Flow440''' recipe==
'''Standby''': N2 purge at 3 SLM and Standby temperature at 440C
'''LM-LOCK''': Check LabManager
'''Wet stabilize''': N2 through bubbler at 1.5 SLM for 20 min and then wait for operator to open the furnace
'''Open'''
'''Load samples'''
'''Close'''
'''Wet oxidation''': Time: variable
'''Open''': Automatically opens after the oxidation time reaches
'''Unload samples'''

Latest revision as of 11:09, 11 May 2023

THIS PAGE IS UNDER CONSTRUCTION

Unless otherwise stated, this page is written by DTU Nanolab internal

The furnace is being tested.

Flow440 recipe

Standby: N2 purge at 3 SLM and Standby temperature at 440C

LM-LOCK: Check LabManager

Wet stabilize: N2 through bubbler at 1.5 SLM for 20 min and then wait for operator to open the furnace

Open

Load samples

Close

Wet oxidation: Time: variable

Open: Automatically opens after the oxidation time reaches

Unload samples