Specific Process Knowledge/Thermal Process/A1 Bor Drive-in furnace: Difference between revisions
No edit summary |
|||
(24 intermediate revisions by 4 users not shown) | |||
Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/A1_Bor_Drive-in_furnace click here]''' | '''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/A1_Bor_Drive-in_furnace click here]''' | ||
''This page is written by DTU Nanolab internal'' | |||
[[Category: Equipment |Thermal A1]] | [[Category: Equipment |Thermal A1]] | ||
Line 7: | Line 9: | ||
==Boron Drive-in | ==Boron Drive-in and Pre-dep furnace (A1)== | ||
[[Image:A1.JPG|thumb| | [[Image:A1.JPG|thumb|400x400px|Boron Drive-in and Pre-dep furnace (A1). Positioned in cleanroom B-1/ Photo: DTU Nanolab internal]] | ||
The Boron Drive-in | The Boron Drive-in and Pre-dep furnace (A1) is a Tempress horizontal furnace for thermal oxidation of silicon wafers. Also boron pre-deposition/doping is done in this furnace. Furthermore, the furnace is used for boron drive-in after the pre-deposition or after boron ion implantation. | ||
The furnace is mostly used for wet and dry thermal oxidation of silicon wafers. The oxidation recipes are named e.g. "WET1000" and "DRY1000", where "WET" or "DRY" indicates whether it is a wet or dry oxidation process, and the number indicates the oxidation temperature. | |||
The purpose of the boron doping is to make conductive structures, etch stop layers etc. For pre-deposition of silicon wafers, boron-nitride source wafers are used as doping source. There are only a few source wafers available, i.e. it is not possible to dope an entire batch of 30 wafers, but both sides of the source wafers are available for doping. It is necessary to activate the source wafers before use by heating them for 1 hour at the temperature needed during the pre-deposition (but never at a temperatures lower than 1050 C). During the pre-deposition a boron phase layer is created on the silicon wafers. This layer can be removed in BHF, if argon is used instead of nitrogen for the pre-deposition (at temperatures higher then 1050 C), otherwise the wafers have to be oxidized before the BHF etch. When the boron phase layer has been removed, the wafers can go directly into the furnace again for a drive-in process with or without an oxide growth. | |||
The Boron Drive-in and Pre-dep furnace is the top furnace tube in the furnace A-stack positioned in cleanroom B-1. The furnaces in the A-stack are the cleanest of all furnaces in the cleanroom. Please be aware of that all wafers have to be RCA cleaned before they enter the furnace, and please check the cross contamination information in LabManager, before you use the furnace. Before boron pre-deposition, also the source wafers and a dedicated carbide boat have to be RCA cleaned. | |||
'''The user manual, quality control instruction and results, technical information and contact information can be found in LabManager:''' | '''The user manual, quality control instruction and results, technical information and contact information can be found in LabManager:''' | ||
'''[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=47 Boron Drive-in | '''[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=47 Boron Drive-in and Pre-dep furnace (A1)]''' | ||
==Process knowledge== | ==Process knowledge== | ||
*Oxidation: look at the [[Specific Process Knowledge/Thermal Process/Oxidation|Oxidation]] page | |||
*Boron drive-in: look at the [[Specific Process Knowledge/Thermal Process/Dope with Boron|Dope with Boron]] page | *Boron drive-in: look at the [[Specific Process Knowledge/Thermal Process/Dope with Boron|Dope with Boron]] page | ||
*Boron doping: look at the [[Specific Process Knowledge/Thermal Process/Dope with Boron|'''Dope with Boron''']] page. | *Boron doping: look at the [[Specific Process Knowledge/Thermal Process/Dope with Boron|'''Dope with Boron''']] page. | ||
<br clear="all" /> | <br clear="all" /> | ||
Line 40: | Line 44: | ||
! QC Recipe: | ! QC Recipe: | ||
! | ! WET1050 | ||
! | ! DRY1050 | ||
|- | |- | ||
| H<sub>2</sub> flow | | H<sub>2</sub> flow | ||
Line 52: | Line 56: | ||
|- | |- | ||
|Temperature | |Temperature | ||
|1050 C | |1050 <sup>o</sup>C | ||
|1050 C | |1050 <sup>o</sup>C | ||
|- | |- | ||
|Oxidation time | |Oxidation time | ||
Line 68: | Line 72: | ||
and over the boat) | and over the boat) | ||
|- | |- | ||
! | !DRY1050 | ||
| | |107.3 nm - 113.3 nm | ||
|3 % | |3.2 % | ||
|- | |- | ||
! | !WET1050 | ||
| | |298.2 nm - 305.5 nm | ||
| | |3.7 % | ||
|- | |- | ||
|} | |} | ||
|- | |- | ||
|} | |} | ||
Numbers from March 2020 | |||
|} | |} | ||
==Overview of the performance of the Boron Drive-in | |||
==Overview of the performance of the Boron Drive-in and Pre-dep furnace and some process related parameters== | |||
{| border="2" cellspacing="0" cellpadding="2" | {| border="2" cellspacing="0" cellpadding="2" | ||
Line 87: | Line 93: | ||
!style="background:silver; color:black;" align="center"|Purpose | !style="background:silver; color:black;" align="center"|Purpose | ||
|style="background:LightGrey; color:black"| | |style="background:LightGrey; color:black"| | ||
* | *Thermal oxidation of Si wafers | ||
* | *Boron pre-deposition/doping of Si wafers | ||
*Oxidation of boron phase layers | *Oxidation of boron phase layers | ||
* | *Driving-in pre-deposited or ion-implanted boron | ||
|style="background:WhiteSmoke; color:black"| | |||
|style="background:WhiteSmoke; color:black"| | Thermal oxidation: | ||
*Dry | *Dry oxidation using O<sub>2</sub> | ||
*Wet | *Wet oxidation using H<sub>2</sub>O vapour | ||
* | Boron pre-deposition/doping: | ||
*Boron-nitride wafers are used as doping source. This is a solid doping source containing B<sub>2</sub>O<sub>3</sub> | |||
Driving-in pre-deposited or ion-implanted boron | |||
*Dry or wet oxidation recipes are normally used for this purpose | |||
|- | |- | ||
!style="background:silver; color:black" align="center"|Performance | !style="background:silver; color:black" align="center"|Performance | ||
|style="background:LightGrey; color:black"|Film thickness||style="background:WhiteSmoke; color:black"| | |style="background:LightGrey; color:black"|Film thickness||style="background:WhiteSmoke; color:black"| | ||
*Dry oxide: | *Dry oxide: ~ 0 nm - 300 nm (it takes too long to grow a thicker oxide) | ||
*Wet oxide: | *Wet oxide: ~ 0 nm - 3 µm (23 hours wet oxidation at 1100 <sup>o</sup>C for Si[100] wafers) | ||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameter range | !style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameter range | ||
Line 109: | Line 118: | ||
|style="background:LightGrey; color:black"|Process pressure | |style="background:LightGrey; color:black"|Process pressure | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*1 atm | *1 atm (no vacuum) | ||
|- | |- | ||
|style="background:LightGrey; color:black"|Gasses on the system | |style="background:LightGrey; color:black"|Gasses on the system | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*N<sub>2</sub> | |||
*O<sub>2</sub>, | *O<sub>2</sub> | ||
*H<sub>2</sub> (in a torch, H<sub>2</sub> and O<sub>2</sub> burns into H<sub>2</sub>O vapour for wet oxidation) | |||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates | !style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates | ||
Line 124: | Line 134: | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*Silicon wafers (RCA cleaned) | *Silicon wafers (RCA cleaned) | ||
*Boron-nitride source wafers for boron pre-deposition/doping | |||
|- | |- | ||
|} | |} |
Latest revision as of 13:40, 31 January 2023
Feedback to this page: click here
This page is written by DTU Nanolab internal
Boron Drive-in and Pre-dep furnace (A1)
The Boron Drive-in and Pre-dep furnace (A1) is a Tempress horizontal furnace for thermal oxidation of silicon wafers. Also boron pre-deposition/doping is done in this furnace. Furthermore, the furnace is used for boron drive-in after the pre-deposition or after boron ion implantation.
The furnace is mostly used for wet and dry thermal oxidation of silicon wafers. The oxidation recipes are named e.g. "WET1000" and "DRY1000", where "WET" or "DRY" indicates whether it is a wet or dry oxidation process, and the number indicates the oxidation temperature.
The purpose of the boron doping is to make conductive structures, etch stop layers etc. For pre-deposition of silicon wafers, boron-nitride source wafers are used as doping source. There are only a few source wafers available, i.e. it is not possible to dope an entire batch of 30 wafers, but both sides of the source wafers are available for doping. It is necessary to activate the source wafers before use by heating them for 1 hour at the temperature needed during the pre-deposition (but never at a temperatures lower than 1050 C). During the pre-deposition a boron phase layer is created on the silicon wafers. This layer can be removed in BHF, if argon is used instead of nitrogen for the pre-deposition (at temperatures higher then 1050 C), otherwise the wafers have to be oxidized before the BHF etch. When the boron phase layer has been removed, the wafers can go directly into the furnace again for a drive-in process with or without an oxide growth.
The Boron Drive-in and Pre-dep furnace is the top furnace tube in the furnace A-stack positioned in cleanroom B-1. The furnaces in the A-stack are the cleanest of all furnaces in the cleanroom. Please be aware of that all wafers have to be RCA cleaned before they enter the furnace, and please check the cross contamination information in LabManager, before you use the furnace. Before boron pre-deposition, also the source wafers and a dedicated carbide boat have to be RCA cleaned.
The user manual, quality control instruction and results, technical information and contact information can be found in LabManager:
Boron Drive-in and Pre-dep furnace (A1)
Process knowledge
- Oxidation: look at the Oxidation page
- Boron drive-in: look at the Dope with Boron page
- Boron doping: look at the Dope with Boron page.
Quality Control - Parameters and Limits
Quality control (QC) for the processes "Wet1050" and "Dry1050" | ||||||||||||||||||||||||||
Numbers from March 2020 |
Purpose |
|
Thermal oxidation:
Boron pre-deposition/doping:
Driving-in pre-deposited or ion-implanted boron
|
---|---|---|
Performance | Film thickness |
|
Process parameter range | Process Temperature |
|
Process pressure |
| |
Gasses on the system |
| |
Substrates | Batch size |
|
Substrate materials allowed |
|