1 July 2024

     16:36  Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4/Slow etch diffhist −10 Bghe talk contribs

28 June 2024

     14:37  Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4/Slow etch diffhist +223 Bghe talk contribs

27 June 2024

     12:44  Specific Process Knowledge/Etch/Wet Titanium Etch diffhist +19 Hvje talk contribs (→‎Comparing the two solutions)