Specific Process Knowledge/Etch/Etching of Titanium
< Specific Process Knowledge | Etch
Jump to navigation
Jump to search
Revision as of 11:11, 11 February 2008 by 192.38.87.73 (talk)
Etching of Titanium
Etching of Titanium is done wet at Danchip making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4 or in the PP-etch bath in the fume hood in cleanroom 2. We have ?:
- BHF
- Cold RCA1 (as stripper)
Comparing the two solutions
BHF | Cold RCA1 | |
---|---|---|
General description |
Etch of titanium with or without photoresist mask. |
Etch of titanium (as stripper) |
Chemical solution | HF:NHF | NH3OH:H2O2:H2O - 1:1:5 |
Process temperature | Room temperature | Room temperature |
Possible masking materials |
Photoresist (1.5 µm AZ5214E) |
None |
Etch rate |
Not known (it bubbles while etching) |
Not known |
Batch size |
1-25 wafers at a time |
1-25 wafer at a time |
Size of substrate |
4" wafers |
4" wafers |
Allowed materials |
No restrictions when used in beaker or PP-etch bath in the fume hood in cleanroom 2. |
|