Etching of Titanium
Etching of titanium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Titanium Etch Metodes
Ti wet etch 1 | Ti wet etch 2 | ICP metal | IBE (Ionfab300+) | |
---|---|---|---|---|
Generel description | BHF:Etch of titanium with or without photoresist mask. | Cold RCA1: Etch of titanium (as stripper or with eagle resist). | Dry plasma etch of Ti | Sputtering of Ti - pure physical etch |
Etch rate range |
|
|
|
|
Etch profile |
|
|
|
|
Substrate size |
|
|
|
Smaller pieces glued to carrier wafer
|
Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
|
|