Specific Process Knowledge/Etch/Etching of Titanium: Difference between revisions
Line 3: | Line 3: | ||
# BHF | # BHF | ||
# Cold RCA1 | # Cold RCA1 | ||
Do it by making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. BHF etching can also take place in the PP-etch bath in the fume hood in cleanroom 2. | Do it by making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. BHF etching can also take place in the PP-etch bath in the fume hood in cleanroom 2. | ||
Line 19: | Line 19: | ||
Etch of titanium with or without photoresist mask. | Etch of titanium with or without photoresist mask. | ||
| | | | ||
Etch of titanium (as stripper) | Etch of titanium (as stripper or with eagle resist). | ||
|- | |- | ||
|'''Chemical solution''' | |'''Chemical solution''' |
Revision as of 10:12, 21 February 2008
Etching of Titanium
Etching of Titanium is done wet at Danchip. We have two solutions for titanium etching:
- BHF
- Cold RCA1
Do it by making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. BHF etching can also take place in the PP-etch bath in the fume hood in cleanroom 2.
Comparing the two solutions
BHF | Cold RCA1 | |
---|---|---|
General description |
Etch of titanium with or without photoresist mask. |
Etch of titanium (as stripper or with eagle resist). |
Chemical solution | HF:NHF | NHOH:HO:HO - 1:1:5 |
Process temperature | Room temperature | Room temperature |
Possible masking materials |
Photoresist (1.5 µm AZ5214E) |
Eagle resist |
Etch rate |
Not known (it bubbles while etching) |
Not known |
Batch size |
1-5 4" in beaker 1-25 wafers at a time in PP-etch bath |
1-5 4" wafer at a time |
Etch bath | Beaker or PP-etch bath in the fume hood in cleanroom 2. | Beaker |
Allowed materials |
No restrictions when used in beaker or PP-etch bath in the fume hood in cleanroom 2. Make a note on the beaker of which materials have been processed. |
No restrictions when used in beaker. Make a note on the beaker of which materials have been processed. |