Specific Process Knowledge/Back-end processing/Die Bonder: Difference between revisions
Jump to navigation
Jump to search
No edit summary |
No edit summary |
||
Line 17: | Line 17: | ||
*[[Specific Process Knowledge/Back-end processing/Au-Sn eutectic die bonding|Au-Sn eutectic die bonding]] | *[[Specific Process Knowledge/Back-end processing/Au-Sn eutectic die bonding|Au-Sn eutectic die bonding]] | ||
== Flip-chip bonder (glue attachment) == | |||
==Equipment performance and process related parameters== | ==Equipment performance and process related parameters== |
Revision as of 16:56, 6 May 2013
Feedback to this page: click here
Die bonder (eutectic metal soldering)
The Cammax EDB80 Die bonder is for placing and soldering dies onto a package or substrate.
The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:
Process information
Flip-chip bonder (glue attachment)
Equipment | Die bonder | Flip-chip bonder | |
---|---|---|---|
Purpose |
|
| |
Performance |
|
| |
Substrates | Allowed materials |
|
|