The Cammax EDB80 Die bonder is for placing and soldering dies onto a package or substrate. | The Cammax EDB80 Die bonder is for placing and soldering dies onto a package or substrate. | ||
[[Image:section under construction.jpg|70px]] ''Will be temporary taken out of service during the PolyFabLab construction.'' | |||
The bonder has a graphite heater element enabling fast heating to the melting point of the solder. To prevent oxidation of the solder and bonding surfaces it is possible to have a gas flow of formier gas (4-10% H2 in N2) over the sample. The machine also has a pick-up tool enabling accurate placement of the sample onto a carrier. | The bonder has a graphite heater element enabling fast heating to the melting point of the solder. To prevent oxidation of the solder and bonding surfaces it is possible to have a gas flow of formier gas (4-10% H2 in N2) over the sample. The machine also has a pick-up tool enabling accurate placement of the sample onto a carrier. |
Latest revision as of 15:59, 6 March 2023
Feedback to this page: click here
Die bonder (eutectic metal soldering)
The Cammax EDB80 Die bonder is for placing and soldering dies onto a package or substrate.
Will be temporary taken out of service during the PolyFabLab construction.
The bonder has a graphite heater element enabling fast heating to the melting point of the solder. To prevent oxidation of the solder and bonding surfaces it is possible to have a gas flow of formier gas (4-10% H2 in N2) over the sample. The machine also has a pick-up tool enabling accurate placement of the sample onto a carrier.
The user manuals, user APVs, technical information and contact information can be found in LabManager:
Process information
Equipment | Die bonder | |
---|---|---|
Purpose |
| |
Performance |
| |
Substrates | Allowed materials |
|