Silicon etching on the ICP Metal Etcher
Unless otherwise stated, all content on this page was created by Jonas Michael-Lindhard, DTU Nanolab
In the primary silicon etcher at Nanolab, the DRIE-Pegasus, silicon is etched using a fluorine based plasma (with SF6 as etch gas). Silicon is also etched by chlorine and bromine.