Specific Process Knowledge/Etch/Etching of Molybdæn

From LabAdviser

THIS PAGE IS UNDER CONSTRUCTION

=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]=


Comparison of Molybdenum Etch Methods

Mo wet etch Specific_Process_Knowledge/Etch/Dry etch
Generel description Wet etch of Pt Sputtering of Pt
Etch rate range
  • ~ 1 - 10 nm/min (not tested yet)
  • ~30nm/min (not tested yet)
Etch profile
  • Isotropic
  • Anisotropic (angles sidewalls, typical around 70 dg)
Masking material
  • None (only used for stripping Pt)
  • Any material that is allowed in the chamber, photoresists included
Substrate size
  • Any size and number that can go inside the beaker in use

Smaller pieces glued to carrier wafer

  • #1 50mm wafer
  • #1 100mm wafer
  • #1 150mm wafer
  • #1 200mm wafer
Allowed materials

No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals

  • Silicon
  • Silicon oxides
  • Silicon nitrides
  • Metals from the +list
  • Metals from the -list
  • Alloys from the above list
  • Stainless steel
  • Glass
  • III-V materials
  • Resists
  • Polymers
  • Capton tape