- 11:45, 22 January 2024 Thope talk contribs created page Specific Process Knowledge/Lithography/EBeamLithography/AR-P 617 (Created page with "AR-P 617 is a positive PMMA based E-beam resist from Allresist. =Spin coating= AR-P 617 can be spin coated on LabSpin 2 and 3 using the CSAR/PMMA bowlset. A spin curve for AR-P 617.06 is provided below. Process parameters are: *Coater: LabSpin 3 *Substrate: 2" Si *Acceleration: 1000 RPM/s Time: 60 s Baking temperature: 200C (setpoint at 222C) Baking time: 120 s")