Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/Warming up time

From LabAdviser
Revision as of 15:21, 6 February 2023 by Rkch (talk | contribs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.

All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.


Laser sources

The laser micromachining tool is equipped with two laser sources (1) picosecond laser (TBW) and (2) a nanosecond laser (IPG). The technical specification provided by the supplier 3D micromac are shown below (as of 1st of Mar 2017 only the picosecond laser can be used \ rkch)

Specifications from 3D micromac

Picosecond (TBW) Nanosecond (IPG)
Wavelength 1064nm, 532nm, 355nm 1064nm
Pulse duration 10ps 120ns
Repetition rate 200 kHz up to 8000 kHz software controlled 200kHz
Output power > 50 W @ 1064 nm 100 W
Warm-up time 25min none