Specific Process Knowledge/Etch/Etching of Silicon Nitride/Etch of Silicon Nitride using RIE
< Specific Process Knowledge | Etch | Etching of Silicon Nitride
Jump to navigation
Jump to search
Revision as of 16:05, 29 October 2007 by BGE (talk | contribs) (New page: For a general introduction to RIE at Danchip see RIE (Reactive Ion Etch) Etching of silicon nitride using RIE can be done with several recipes. It can be etched by our standard silic...)
For a general introduction to RIE at Danchip see RIE (Reactive Ion Etch)
Etching of silicon nitride using RIE can be done with several recipes. It can be etched by our standard silicon etch recipe: OH_PolyA which is based on SF6. It can also be etched using the recipe 1Nitride which is based on CHF3. The difference of these two etches has not been investigate in details. Look in the table below to see what we know