Etch of SiO2 using the recipe 1SIO2mbr with burned resist as masking material, by Berit Geilman Herstrøm (BGE) from Danchip@DTU

Process date: Before 2004
Recipe: 1sio2mbr
Process time: ? min
Mask: Burned resist
Structure size on mask: 3 µm
Etch rate ~120nm/min