Warning: This file type may contain malicious code. By executing it, your system may be compromised.

AFM picture of Cr layer deposited with E-beam evaporation in Wordentec. Deposition rate 10 Å/s.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeDimensionsUserComment
current15:34, 12 August 2008 (174 KB)Kn (talk | contribs)AFM picture of e-beam deposited Cr layer, deposited with Wordentec. Rate 1 nm/s.
15:29, 12 August 2008 (174 KB)Kn (talk | contribs)AFM picture of Cr layer deposited with E-beam evaporation in Wordentec. Deposition rate 10 Å/s.