Template:Spinning KS Spinner: AZ

From LabAdviser
Revision as of 10:46, 6 March 2008 by BGE (talk | contribs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

KS Spinner is the other option for spinning the standard thicknesses.

  • 1.5µm resist use the recipe: Danchip_1.5um_4"and6"
  • 2.2µm resist use the recipe: Danchip2_2_4"

Please see the parameters for these recipes and some other suggestions in this document:Thin resist parameters