Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using AOE/Standard recipe with resist mask/Striation
< Specific Process Knowledge | Etch | Etching of Silicon Oxide | SiO2 etch using AOE | Standard recipe with resist mask
Jump to navigation
Jump to search
Feedback to this page: click here
Striation: Side wall roughness
Sidewall roughness and resist surface after etch viewed with SEM
- Striation with different resists used
Roughness of the resist after etch measured with the AFM