Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using AOE/Standard recipe with resist mask/Variations over SiO2 mres

From LabAdviser
< Specific Process Knowledge‎ | Etch‎ | Etching of Silicon Oxide‎ | SiO2 etch using AOE‎ | Standard recipe with resist mask
Revision as of 12:58, 19 November 2015 by Bghe (talk | contribs) (Created page with "'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etc...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

Feedback to this page: click here

Experiments done with the TDESC electrode that we installed in 2010 (by Roy and Berit)

After changing the electrode to the TDESC type we got a lot of issues with trenching during the acceptance test. After doing a lot of experiments and optimization it turned out that this was probably do to a bad resist profile. We used a negative resist and the problems were gone. Here I show some of the results we got during this optimization.

Conclusions

  • Very important to have a good resist profile before etch.
  • Trenching and rounded corners can be controlled with coil and platen power.
  • H2 does not have much influence (expected to have influence on the SiO2:Si selectivity)
  • C4F8 flow has a influence on the profile and on the aspect ratio dependent etch - keep it low.
  • Pressure does not show much influence