Specific Process Knowledge/Thin film deposition/Deposition of Aluminium Nitride

From LabAdviser
Revision as of 10:10, 7 October 2015 by Paphol (talk | contribs) (Created page with "=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>200px= '''Feedback to this page''': '''[mailto:labadviser@danchip.dt...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

THIS PAGE IS UNDER CONSTRUCTION

Feedback to this page: click here


Deposition of MgB

Write a short description of the process and how to perform the process.



Only one method at the moment

Cryofox PVD co-sputter/evaporation
Generel description
  • Reactive Co-Sputtering
Stoichiometry
  • Depend on the targets power
Film Thickness
  • 0nm - 200nm
Deposition rate
  • Not tested
Step coverage
  • Very good
Process Temperature
  • Up to 400oC
Substrate size
  • 100 mm wafers (Up to 12 wafers at a time)
  • 150 mm wafers (Up to 4 wafers at a time)
Allowed materials
  • Silicon
  • Silicon oxide, silicon nitride
  • Quartz/fused silica
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Any metals