Lyngby 20.6.11

All Layers:
	5" chromium mask
	Soda-lime Glass
	Dark periphery
	Chromium up

CIF-file: MyMask.cif

Top cell: Wafer  
Layer: MT1 
Mask Type: Clear field, wrong reading
Text: DTU PicoTech - Nancy Noname - jun 11 - Front mask

CIF-file: MyMask.cif

Top cell: Wafer
Layer: MT2
Mask Type: Dark field, right reading
Text: DTU PicoTech - Nancy Noname - jun 11 - Back mask