Specific Process Knowledge/Etch/Etching of Aluminium

From LabAdviser

Etching of Aluminium

Etching of aluminium is done wet at Danchip. We have two different solutions:

(1) H2O:H3PO4 1:2 at 50 oC (2) Pre-mixed etch solution: PES 77-19-04 at 20 oC