- 12:18, 20 May 2016 Eves talk contribs uploaded File:XPS depth Al 10 Ti.jpg (MsUpload)
- 17:53, 19 May 2016 Eves talk contribs uploaded a new version of File:Al2O3 TiO2 flat multilayers.jpg (MsUpload)
- 17:51, 19 May 2016 Eves talk contribs uploaded File:Al2O3 TiO2 flat multilayers 22.jpg (MsUpload)
- 17:49, 19 May 2016 Eves talk contribs uploaded File:Al2O3 TiO2 flat multilayers 2.jpg (MsUpload)
- 17:47, 19 May 2016 Eves talk contribs uploaded a new version of File:Al2O3 TiO2 flat multilayers.jpg (MsUpload)
- 17:45, 19 May 2016 Eves talk contribs uploaded File:Al2O3 TiO2 flat multilayers.jpg (MsUpload)
- 17:26, 19 May 2016 Eves talk contribs uploaded File:TiO2 LT Thickness.JPG (MsUpload)
- 17:26, 19 May 2016 Eves talk contribs uploaded File:TiO2 LT RI.JPG (MsUpload)
- 17:04, 19 May 2016 Eves talk contribs uploaded File:Al2O3 LT Thickness.JPG (MsUpload)
- 17:04, 19 May 2016 Eves talk contribs uploaded File:Al2O3 LT RI.JPG (MsUpload)
- 15:48, 19 May 2016 Eves talk contribs uploaded File:Evgeniy Shkondin Si trenches coverd with Al2O3 and TiO2 multilayers using ALD.JPG (MsUpload)
- 10:47, 19 May 2016 Eves talk contribs uploaded a new version of File:HT Al2O3 Carbon content.JPG (MsUpload)
- 10:47, 19 May 2016 Eves talk contribs uploaded a new version of File:LT Al2O3 Carbon content.JPG (MsUpload)
- 10:47, 19 May 2016 Eves talk contribs uploaded a new version of File:HT Al2O3 Carbon content.JPG (MsUpload)
- 10:47, 19 May 2016 Eves talk contribs uploaded a new version of File:LT Al2O3 Carbon content.JPG (MsUpload)
- 15:59, 18 May 2016 Eves talk contribs uploaded a new version of File:HT Al2O3 Carbon content.JPG (MsUpload)
- 15:59, 18 May 2016 Eves talk contribs uploaded a new version of File:LT Al2O3 Carbon content.JPG (MsUpload)
- 15:55, 18 May 2016 Eves talk contribs uploaded a new version of File:HT Al2O3 Carbon content.JPG (MsUpload)
- 15:55, 18 May 2016 Eves talk contribs uploaded a new version of File:LT Al2O3 Carbon content.JPG (MsUpload)
- 15:42, 18 May 2016 Eves talk contribs uploaded File:HT Al2O3 Carbon content.JPG (MsUpload)
- 15:42, 18 May 2016 Eves talk contribs uploaded File:LT Al2O3 Carbon content.JPG (MsUpload)
- 16:15, 17 May 2016 Eves talk contribs uploaded File:SE Al2O3 TiO2 150C typical.JPG (MsUpload)
- 16:15, 17 May 2016 Eves talk contribs uploaded File:SE Al2O3 TiO2 350C typical.JPG (MsUpload)
- 15:19, 17 May 2016 Eves talk contribs uploaded a new version of File:Al2O3 O3 300C.JPG (MsUpload)
- 15:07, 17 May 2016 Eves talk contribs uploaded File:SE Al2O3 ALD O3 300C typical.JPG (MsUpload)
- 15:07, 17 May 2016 Eves talk contribs uploaded File:Al2O3 O3 350C.JPG (MsUpload)
- 15:07, 17 May 2016 Eves talk contribs uploaded File:Al2O3 O3 300C.JPG (MsUpload)
- 15:07, 17 May 2016 Eves talk contribs uploaded File:SE Al2O3 ALD O3 350C typical.JPG (MsUpload)
- 10:18, 17 May 2016 Eves talk contribs uploaded File:SE Al2O3 ALD typical.JPG (MsUpload)
- 18:18, 16 May 2016 Eves talk contribs uploaded File:TiO2T whole.jpg (MsUpload)
- 18:18, 16 May 2016 Eves talk contribs uploaded File:TiO2T top2.jpg (MsUpload)
- 18:18, 16 May 2016 Eves talk contribs uploaded File:TiO2T top1.jpg (MsUpload)
- 18:18, 16 May 2016 Eves talk contribs uploaded File:TiO2T middle.jpg (MsUpload)
- 18:18, 16 May 2016 Eves talk contribs uploaded File:TiO2T bottom2.jpg (MsUpload)
- 18:18, 16 May 2016 Eves talk contribs uploaded File:TiO2T bottom1.jpg (MsUpload)
- 17:51, 16 May 2016 Eves talk contribs uploaded File:TiO2 XPS results Cl.JPG (MsUpload)
- 17:51, 16 May 2016 Eves talk contribs uploaded File:TiO2 XPS results.JPG (MsUpload)
- 17:07, 16 May 2016 Eves talk contribs uploaded File:TiO2 300C.jpg (MsUpload)
- 17:06, 16 May 2016 Eves talk contribs uploaded File:TiO2 250C.jpg (MsUpload)
- 17:06, 16 May 2016 Eves talk contribs uploaded File:TiO2 150C.jpg (MsUpload)
- 17:06, 16 May 2016 Eves talk contribs uploaded File:TiO2 350C.jpg (MsUpload)
- 15:21, 16 May 2016 Eves talk contribs uploaded File:Al2O3T top2.jpg (MsUpload)
- 15:21, 16 May 2016 Eves talk contribs uploaded File:Al2O3T top1.jpg (MsUpload)
- 15:21, 16 May 2016 Eves talk contribs uploaded File:Al2O3T middle.jpg (MsUpload)
- 15:21, 16 May 2016 Eves talk contribs uploaded File:Al2O3T bottom2.jpg (MsUpload)
- 15:21, 16 May 2016 Eves talk contribs uploaded File:Al2O3T bottom1.jpg (MsUpload)
- 15:21, 16 May 2016 Eves talk contribs uploaded File:Al2O3T whole.jpg (MsUpload)
- 10:53, 16 May 2016 Eves talk contribs uploaded File:Al2O3 XPS.jpg (MsUpload)
- 10:38, 16 May 2016 Eves talk contribs uploaded a new version of File:ALD window.jpg (MsUpload)
- 10:34, 16 May 2016 Eves talk contribs uploaded File:ALD window.jpg