Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using ASE/More test with CF4/H2, CHF3 and C4F8/H2 - SiO2 etch
< Specific Process Knowledge | Etch | Etching of Silicon Oxide | SiO2 etch using ASE
Jump to navigation
Jump to search
Revision as of 13:46, 14 December 2023 by Mfarin (talk | contribs) (→Recipes and results - C4F8 / H2 tests)
More test with CF4/H2, CHF3 and C4F8/H2 - SiO2 etch
Tests performed by Maria Farinha @DTU Nanolab
Recipes and results - CF4 / H2 tests