Both RIE's (RIE1 and RIE2) for silicon based etching has been decommissioned

Etch of SiO2 using the recipe 1SIO2mbr with burned resist as masking material

Berit Geilman Herstrøm (BGE) from Nanolab@DTU

Process date: Before 2004
Recipe: 1sio2mbr
Process time: ? min
Mask: Burned resist
Structure size on mask: 3 µm
Etch rate ~120nm/min