Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
9/9-2014 6" First DUV box wafer standard stepper mask (50 nm barc + 320 nm krf) Si / 50%+ ICP Metal Etch / jmli 2*30 sec barc etch using 'slow etch with carrier' isoslow1 , 2:00 minutes S005292