Template:Spinning KS Spinner: AZ
KS Spinner is the other option for spinning the standard thicknesses.
- 1,5 um resist use the recipe: Danchip_1,5um_4"and6"
- 2,2 um resist use the recipe: Danchip2_2_4"
Please see the parameters for these recipes and some other suggestions in this document:Thin resist parameters