Specific Process Knowledge/Etch/Etching of TOPAS

From LabAdviser

Etching of TOPAS

TOPAS is etched by an oxygen plasma in the ASE. Masking of TOPAS was achieved by photo resist or a hard mask of aluminum or silicon. Photo resist is the preferred masking material, since hard masks tends to introduce local masking due to redeposition. TOPAS can be etched at rates up to 500 nm/min, with excellent uniformity over the wafer.

TOPAS by khara@danchip
Parameter TOPAS etch
O2 (sccm) 99
CO2 (sccm) 0
Pressure (mTorr) 40
Coil power (W) 720
Platen power (W) 60
Temperature (oC) 20
Etch rate (nm/min) ~500