Specific Process Knowledge/Etch/AOE (Advanced Oxide Etch)/Silicon Nitride Etch using AOE/Nitride etch with DUV mask
Feedback to this page: click here
Silicon nitride etch with STS recommended silicon nitride recipe
Silicon nitride etch with the standard silicon oxide etch
-
Profile of lines with 1µm pitch
-
Profile of lines with 4µm pitch
-
Profile of 2µm line - zoom in on 4µm pitch