Molybdenum deposition

Molybdenum can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.

E-beam evaporation (Alcatel) E-beam evaporation (PVD co-sputter/evaporation) Sputter deposition (Lesker)
General description E-beam deposition of Mo E-beam deposition of Mo Sputter deposition of Mo
Pre-clean RF Ar clean RF Ar clean RF Ar clean
Layer thickness 10Å to 0.5 µm* 10Å to 500 Å 10Å to 500 Å
Deposition rate 2Å/s to 15Å/s About 1 Å/s Depends on process parameters, roughly about 1 Å/s
Batch size
  • Up to 1x4" wafers
  • smaller pieces
  • 12x2" wafers or
  • 12x4" wafers or
  • 4x6" wafers
  • Pieces or
  • 1x4" wafer or
  • 1x6" wafer
Allowed materials
  • Silicon
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
  • Silicon
  • Silicon oxide
  • Silicon nitride
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Silicon
  • Silicon oxide
  • Silicon nitride
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
Comment Only very thin layers (up to 100nm).


* For thicknesses above 200 nm permission from ThinFilm group (thinfilm@danchip.dtu.dk) is required.