Specific Process Knowledge/Direct Structure Definition
Feedback to this page: click here
Direct Structure Definiton
By direct structure definition we mean that you form the structures for you device directly in the material that the device consist of without any masking steps. Some of the techniques may require a master.
Choose method of structuring/equipment
- 2-Photon Polymerization Lithography
- Polymer Injection Molder
- Nano Imprint Lithography
- Laser Micromachining Tool/ablation
- Dicing saw
Materials for structuring
- Polymers
- Metals/Silicon/Graphene
- Glass
Comparison of equipment/material
- prøveformat/størrelse
- forudsætninger
- mønsterdannelse
- throughput
- min/max featuresize
- min/max aspect-ratio
- post-treatment
- degree of freedom
Polymers | Nano Imprint Lithography | 2-Photon Polymerization Lithography | Polymer Injection Molder | Laser Micromachining Tool |
---|---|---|---|---|
Generel description | Low Pressure Chemical Vapour Deposition (LPCVD furnace process) | Plasma Enhanced Chemical Vapour Deposition (PECVD process) | Reactive sputtering | |
Allowed materials |
Processed wafers have to be RCA cleaned |
|
Any |
Metals/Silicon/Glass | Nano Imprint Lithography | 2-Photon Polymerization Lithography | Polymer Injection Molder | Laser Micromachining Tool |
---|---|---|---|---|
Generel description | Low Pressure Chemical Vapour Deposition (LPCVD furnace process) | Plasma Enhanced Chemical Vapour Deposition (PECVD process) | Reactive sputtering | |
Allowed materials |
Processed wafers have to be RCA cleaned |
|
Any |